YHH-03A Mine cable-sheath rubber compound
FOB Reference Price / Min.Order Quantity
: Get Latest Prices
Processing Time:1 Days - 60 Days
Packaging Details:
STANDARD EXPORTING PACKAGE
Port: Shanghai / Shenzhen / Qingdao / Ningbo / Other
Payment Terms: L/C , T/T , other
The product meet the standards of the implementation of the documents MT818, and the XH-03A in the GB7594.7-1987.
The colored sheath using imported pigment, production finally ceased cable inside the pipeline does not change color, bright does not fade.
Performance comparison
|
Test item
|
Unit
|
GB7594.7-87
|
Test value
|
|
Before ageing
|
Tensile strength
|
Intermediate values
|
MPa
|
≥11.0
|
13.8
|
|
Elongation at
|
Intermediate values
|
%
|
≥250
|
450
|
|
Heat ageing test of air box
|
Aging conditions
|
Temperature
|
℃
|
75±2
|
|
Time
|
h
|
10×24
|
|
Tensile strength
|
Intermediate values
|
MPa
|
—
|
13.1
|
|
Rate of change
|
%
|
≤-15
|
-5
|
|
Elongation at
|
Intermediate values
|
%
|
≥200
|
420
|
|
Rate of change
|
%
|
≤-25
|
-7
|
|
Hot set test
|
Test conditions
|
Test temperature
|
℃
|
200±3
|
|
Load time
|
min
|
15
|
|
Mechanical stress
|
MPa
|
0.2
|
|
Load elongation
|
%
|
≤175
|
40
|
|
Permanent deformation after cooling
|
%
|
≤25
|
10
|
|
Oil test
|
Test conditions
|
Oil temperature
|
℃
|
100±2
|
|
Dipping oil
|
h
|
24
|
|
Tensile strength
|
Rate of change
|
%
|
≤-40
|
-6
|
|
Elongation at
|
Rate of change
|
%
|
≤-40
|
-10
|
|
Tear resistant test
|
Tearing strength
|
Intermediate values
|
N/mm
|
≥5.0
|
8.5
|

Panjin Yihe Plastic&Rubber Co., Ltd
Basic Information
Business Type:
Main Products:
Location:
Total Employees:
Year Established:
Trade Information
Top 3 Markets:
Accepted Payment Currency:
Nearest Port:
Average Lead Time:
Overseas Office: No
Company Pictures
Verified Supplier
Credit Check